MSK-HRP-300 (updated from MSK-H2150-RP300) is a special Roll-to-Plate hot press with a working temperature of up to 200°C. The hot roll drives a hot pate via DC motor to achieve flat pressing, which is designed for better laminating multilayer materials
SPECIFICATIONS:
| Power |
- 208-240 VAC, 50/60 Hz, single phase, 20 A
- 4.5 kVA
|
Roller Material & Size

|
- High strength refractory steel with hardness RC > 58
- Roller Size: 96 mm Dia. x 220mm W (4" D x 8"W)
- Suggested rolling width: 150 mm
- Roll line speed: 0~ 50 mm/s adjustable
- Max. the temperature for the roller: 200°C
- Driving by DC motor
- Ar gas glove box compatible
|
|
Roller Gap ( Thickness )
|
|
|
Dial Gauge Accuracy (Thickness Indicating )
|
- Dual digital micrometer heads
- Accuracy: +/- 0.005mm
|
|
Movable Hot Plate
|
- The hot plate is made of High strength refractory steel with hardness RC > 58
- Dimension: 200 mm W x 300 mm L
- The hot plate is movable by the hot roller via friction
- Max. working temperature: 300°C
-
Water chiller is required but not included if the working temperature is > 100°C
- Max. Rolling width on the plate: 150mm
|
|
Heating Temperature
|
- Two digital temperature controllers for control hot roller and hot plate separately
- 200°C suggested, and 300°C maximum
- Max Heating Rate: 4°C/minute
- Temperature Control Accuracy: +/-3°C
|
|
Motor (Ar Gas Glove Box Compatible)
|
- High torque 24VDC motor with reducing gear (1:75)
- Motor power: 40W
- Rolling speed adjustable: 5~45 r/min
|
|
Output Thickness
|
- Depending on the electrode's material and thickness, typically:
- A 0.16mm thick electrode coated on copper can be pressed into a minimum thickness of 0.1 mm
- A 0.06mm thick electrode coated on copper can be pressed into a minimum thickness of 0.04 mm
- A 0.33mm thick silver/gold can be pressed into a minimum thickness of 0.03 mm
- Thickness uniformity: +/- 2 microns if coating electrode thickness +/- 5 micron and each rolling increased < 10 microns
|
| Compliance |
- CE Certified
- NRTL or CSA certification is available upon request at extra cost
|
| Warnings |
- Do not touch the surface of the rolling part of the machine when the rollers are heated up or running
-
You may calibrate the temperature by TC-calibrator-LD, and refer to the instruction here from time to time to ensure heating temperature accuracy
- Multi-step thickness calendaring needed: While calendaring the sample sheet, make each calendaring decrement of 0.02mm compared with the sheet's original thickness
|